包頭2號礦體選冶經濟高效流程的開發

New Combined Process of Niobium Enrichment from No.2 Ore Body of Baotou Niobium-Bearing Iron Ore

  • 摘要: 采用包頭2號礦體的重選粗精礦(含Nb2O51.6%~1.8%),用磁化焙燒-磁選,交流等離子冶煉工藝流程,可獲得低磷中級鈮鐵(含鈮22%~32%,Nb/P>30),鈮收率61.l%.同時獲得含鈮鐵精礦(TFe>60%,Nb2O5~1.0%),流程短效率高而經濟。

     

    Abstract: A new combined magnetizing roasting-separation-smelting process of niobium enrichment from No.2 ore body of Baotou niobium-bearing iron ore has been developed. Using magnetizing roasting-magnetic separation-plasma smelting, a kind of middle grade ferroniobium of 22%~32% Nb and Nb/P>30 has been obtained and total niobium recovery ratio is 61.l%. This combined process has great economical potential because of its shorter flowsheet and more efficient operation.

     

/

返回文章
返回
<span id="fpn9h"><noframes id="fpn9h"><span id="fpn9h"></span>
<span id="fpn9h"><noframes id="fpn9h">
<th id="fpn9h"></th>
<strike id="fpn9h"><noframes id="fpn9h"><strike id="fpn9h"></strike>
<th id="fpn9h"><noframes id="fpn9h">
<span id="fpn9h"><video id="fpn9h"></video></span>
<ruby id="fpn9h"></ruby>
<strike id="fpn9h"><noframes id="fpn9h"><span id="fpn9h"></span>
www.77susu.com